| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 34.80% | 1.00 | |
| B2O3 | 65.20% | 1.51 | |
| Oxide Weight | 161.21 | ||
| Formula Weight | 161.21 | ||
| Materials |
Eutectics
|
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |
| Frit Softening Point | 990C |
|---|