Na Metaborate and Na Metasilicate Eutectic

Oxide Analysis Formula Tolerance
Na2O 48.90% 1.00
SiO2 27.10% 0.57
B2O3 24.00% 0.44
Oxide Weight 126.79
Formula Weight 126.79

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 815C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy