| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| MgO | 26.60% | 1.00 | |
| Al2O3 | 33.60% | 0.50 | |
| SiO2 | 39.80% | 1.00 | |
| Oxide Weight | 151.50 | ||
| Formula Weight | 151.50 | ||
| Materials |
Eutectics
|
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |
| Typecodes |
Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content. |
| Frit Softening Point | 1330C |
|---|