Formula: (NH4)6Mo7O24.4H2O
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| MoO3 | 81.55% | 1.00 | |
| LOI | 18.44% | n/a | |
| Oxide Weight | 143.94 | ||
| Formula Weight | 176.48 | ||
CAS Number: 12054-85-2
Merck Number: 14,533
UN Number: UN3288
Substance is listed in Toxic Substance Control Act (TSCA) inventory.
This decomposes in stages, finally liberating MoO3
| Hazards |
Molybdenum Compounds Toxicology
|
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |
| Frit Softening Point | 190C |
|---|---|
| Density (Specific Gravity) | 2.498 |