Formula: 3.8Na2SiO3 . CaSiO3
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 49.80% | 1.00 | |
| CaO | 9.60% | 0.21 | |
| Na2O | 40.60% | 0.79 | |
| Oxide Weight | 121.07 | ||
| Formula Weight | 121.07 | ||
| Glossary |
Eutectic
In ceramics, this term refers to certain chemistries that melt at much-lower-than-expected temperatures. |
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |
| Frit Softening Point | 932C |
|---|