May 2026: We are continuing a major code rewrite. Please contact us if you find issues. Thank you.
Alternate Names: Fusion Frit F582
Description: Lithium low fire clear frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Li2O | 3.50% | 0.34 | |
| K2O | 2.50% | 0.08 | |
| Na2O | 6.00% | 0.28 | |
| CaO | 5.70% | 0.30 | |
| Al2O3 | 7.20% | 0.21 | |
| B2O3 | 15.60% | 0.65 | |
| SiO2 | 59.50% | 2.89 | |
| Oxide Weight | 292.08 | ||
| Formula Weight | 292.08 | ||
| URLs |
http://www.fusionceramics.com/
Fusion Ceramics Frit Website |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 8.5 x 10-6 |
|---|---|
| Frit Softening Point | 1400F |