Alternate Names: Fusion Frit F562
Description: Alkali boron frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 3.60% | 0.16 | |
| Na2O | 12.26% | 0.83 | |
| CaO | 0.16% | 0.01 | |
| Al2O3 | 17.05% | 0.70 | |
| B2O3 | 29.83% | 1.79 | |
| SiO2 | 37.09% | 2.58 | |
| Oxide Weight | 418.70 | ||
| Formula Weight | 418.70 | ||
| URLs |
http://www.fusionceramics.com/
Fusion Ceramics Frit Website |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 9.06 x 10-6 |
|---|---|
| Frit Melting Range (C) | 1450F |