Alternate Names: Fusion Frit F537
Description: Zinc free high calcium matte frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 2.00% | 0.06 | |
| CaO | 28.00% | 0.94 | |
| Al2O3 | 3.00% | 0.06 | |
| B2O3 | 10.00% | 0.27 | |
| SiO2 | 57.00% | 1.78 | |
| Oxide Weight | 188.19 | ||
| Formula Weight | 188.19 | ||
| URLs |
http://www.fusionceramics.com/
Fusion Ceramics Frit Website |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 7.7 x 10-6 |
|---|---|
| Frit Softening Point | >1850F |