Fusion Frit FZ-647

Alternate Names: Frit FZ647, Frit FZ 647

Oxide Analysis Formula Tolerance
ZnO 20.00% 0.48
PbO 60.00% 0.52
SiO2 20.00% 0.65
Oxide Weight 194.36
Formula Weight 194.36

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.