Alternate Names: Frit FZ583
Description: Barium Zinc Zero Boron frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| BaO | 37.00% | 0.50 | |
| ZnO | 16.00% | 0.41 | |
| SiO2 | 40.00% | 1.39 | |
| Al2O3 | 4.00% | 0.08 | |
| Na2O | 1.50% | 0.05 | |
| K2O | 1.50% | 0.03 | |
| Oxide Weight | 209.19 | ||
| Formula Weight | 209.19 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |