Solargil Frit FR10

Description: Calcium borate low alumina frit

Oxide Analysis Formula Tolerance
K2O 6.58% 0.17
Na2O 5.10% 0.20
MgO 3.15% 0.19
CaO 10.14% 0.44
Al2O3 5.03% 0.12
B2O3 22.32% 0.78
SiO2 47.67% 1.93
Oxide Weight 243.27
Formula Weight 243.27

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 77.4 x 10-7 C (Appen)
Frit Softening Point 980-1020 C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy