Description: Boro alkaline frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 10.07% | 0.40 | |
| Na2O | 9.94% | 0.60 | |
| B2O3 | 29.97% | 1.61 | |
| Al2O3 | 6.00% | 0.22 | |
| SiO2 | 44.02% | 2.74 | |
| Oxide Weight | 374.22 | ||
| Formula Weight | 374.22 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 93.4 x 10-7 C (Appen) |
|---|---|
| Frit Softening Point | 800-950C |