Description: High zinc, zero-alumina frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| MgO | 4.87% | 0.17 | |
| K2O | 14.06% | 0.21 | |
| Na2O | 7.49% | 0.17 | |
| ZnO | 26.61% | 0.46 | |
| SiO2 | 46.98% | 1.09 | |
| Oxide Weight | 139.33 | ||
| Formula Weight | 139.33 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 113.6 x 10-7 C (Appen) |
|---|---|
| Frit Softening Point | 1000-1300C |