June 2026: We are continuing a major code rewrite. Please contact us if you find issues. Thank you.
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| MgO | 3.50% | 0.52 | |
| CaO | 4.10% | 0.43 | |
| TiO2 | 1.20% | 0.09 | |
| Al2O3 | 32.60% | 1.90 | |
| P2O5 | 1.20% | 0.05 | |
| SiO2 | 47.50% | 4.69 | |
| Fe2O3 | 9.90% | 0.37 | |
| Oxide Weight | 593.86 | ||
| Formula Weight | 593.86 | ||
A sample analysis from Ababi Sharon
| Typecodes |
Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |