May 2026: We are continuing a major code rewrite. Please contact us if you find issues. Thank you.
Alternate Names: 1047 Boraksfritte
Description: Calcium borate frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 10.79% | 0.56 | |
| K2O | 2.41% | 0.07 | |
| Na2O | 7.91% | 0.37 | |
| Al2O3 | 17.85% | 0.51 | |
| B2O3 | 20.41% | 0.85 | |
| SiO2 | 40.63% | 1.96 | |
| Oxide Weight | 289.44 | ||
| Formula Weight | 289.44 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |