Description: From Ron Roy's MDT
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.30% | 0.04 | |
| MgO | 0.10% | 0.02 | |
| Al2O3 | 15.00% | 1.00 | |
| SiO2 | 74.00% | 8.37 | |
| Fe2O3 | 10.60% | 0.45 | |
| Oxide Weight | 680.00 | ||
| Formula Weight | 680.00 | ||
| Materials |
Ochre
|
| Typecodes |
Colorant
Metallic based materials that impart fired color to glazes and bodies. |