Description: Sodium/potassium/calcium Feldspar
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 1.40% | 0.14 | |
| K2O | 4.10% | 0.24 | |
| Na2O | 6.82% | 0.62 | |
| Al2O3 | 18.92% | 1.04 | |
| SiO2 | 68.15% | 6.35 | |
| Fe2O3 | 0.06% | - | |
| LOI | 0.08% | n/a | |
| Oxide Weight | 557.21 | ||
| Formula Weight | 557.65 | ||
Used as an alumina source in glass batch formulations. Beneficiated using the froth flotation process for low iron oxide content.
| Materials |
G-200 Feldspar
|
| Materials |
NC-4 Feldspar
|
| Materials |
Calcium Feldspar
|
| Materials |
Potash Feldspar
A feldspar having a KNaO content that predominates in potassium. |
| Materials |
Soda Feldspar
A feldspar having a KNaO content that predominates in sodium. |
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |
| Bulk Density lbs/cu. ft. (Packed) | 80 |
|---|
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk