James Bay Stn Kaolin

Alternate Names: JamesBay Stn

Oxide Analysis Formula Tolerance
Fe2O3 1.20% 0.03
SiO2 55.20% 3.30
P2O5 0.15% -
Al2O3 28.36% 1.00
TiO2 1.12% 0.05
Na2O 0.05% -
K2O 0.45% 0.02
MgO 0.19% 0.02
CaO 0.28% 0.02
LOI 13.00%n/a
Oxide Weight 312.91
Formula Weight 359.66

Related Information

Links

Materials Kaolin
The purest of all clays in nature. Kaolins are used in porcelains and stonewares to impart whiteness, in glazes to supply Al2O3 and to suspend slurries.
Typecodes Kaolin
Pure clay mineral, there are many brand names of varying purity and iron content.