Alternate Names: Clinchfield 202
Description: Legacy potash feldspar
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.20% | 0.02 | |
| K2O | 10.80% | 0.72 | |
| Na2O | 2.50% | 0.25 | |
| Al2O3 | 17.00% | 1.05 | |
| SiO2 | 69.00% | 7.24 | |
| Fe2O3 | 0.10% | - | |
| LOI | 0.30% | n/a | |
| Oxide Weight | 628.24 | ||
| Formula Weight | 630.13 | ||
| Materials |
Potash Feldspar
A feldspar having a KNaO content that predominates in potassium. |
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |