Frit 1510

Description: Netherland, Flanders area (Ferro?)

Oxide Analysis Formula Tolerance
CaO 0.31% 0.01
K2O 2.92% 0.07
Na2O 19.73% 0.69
ZnO 8.77% 0.23
Al2O3 3.16% 0.07
SiO2 65.11% 2.34
Oxide Weight 216.22
Formula Weight 216.22

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.