Frit 1209

Description: Calcium borate frit with very low alumina, silica

Oxide Analysis Formula Tolerance
CaO 40.70% 1.00
B2O3 50.50% 1.00
Al2O3 2.20% 0.03
SiO2 6.50% 0.15
Oxide Weight 137.70
Formula Weight 137.70

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.