Cerium Oxide

Alternate Names: CeO2, Cerium Dioxide

Oxide Analysis Formula Tolerance
CeO2 100.00% 1.00
Oxide Weight 172.11
Formula Weight 172.11

Notes

A colorant used in ceramic glazes. It is a powerful flux. Commercial products have fairly high purity.
Can be used as a polishing and descratching agent for glass.
Also available as a carbonate (CeCO3).

Related Information

Links

URLs http://www.kemcointernational.com/CeriumOxide.htm
Kemco International - Cerium Description
URLs http://en.wikipedia.org/wiki/Cerium_Oxide
Cerium oxide at Wikipedia
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.
Oxides CeO2 - Cerium Oxide
Minerals Bastnäsite
A cerium cortaining carbonate-fluoride mineral.
Minerals Monazite
A cerium containing phosphate mineral.

Data

Hardness (Moh) 6
Frit Softening Point 2500C
Density (Specific Gravity) 7.3

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy