Ferro Frit 3464

Oxide Analysis Formula Tolerance
CaO 11.00% 0.50
PbO 44.10% 0.50
Al2O3 4.00% 0.10
B2O3 5.50% 0.20
SiO2 35.40% 1.50
Oxide Weight 254.03
Formula Weight 254.03

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Materials Hommel Frit 381
Typecodes Leaded Frit
Frits can contain 1% or 80% PbO so this category can be misleading, check the chemistry to find out.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.

Data

Co-efficient of Linear Expansion 7.0
Frit Melting Range (C) 1500F