Burnt Sienna

Description: A very high iron ochre

Oxide Analysis Formula Tolerance
CaO 1.00% 0.61
Al2O3 3.00% 1.00
SiO2 19.00% 10.75
Fe2O3 72.00% 15.30
H2O 5.00%n/a
Oxide Weight 3,230.00
Formula Weight 3,400.00

Related Information

Links

Materials Raw Sienna
Typecodes Clay Other
Clays that are not kaolins, ball clays or bentonites. For example, stoneware clays are mixtures of all of the above plus quartz, feldspar, mica and other minerals. There are also many clays that have high plasticity like bentonite but are much different mineralogically.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy