| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Li2O | 4.30% | 0.95 | |
| Na2O | 0.50% | 0.05 | |
| Al2O3 | 17.50% | 1.13 | |
| SiO2 | 77.00% | 8.41 | |
| LOI | 0.70% | n/a | |
| Oxide Weight | 651.75 | ||
| Formula Weight | 656.34 | ||