Pearl Ash Calcined

Alternate Names: Potash Calcined, Calcined Potash

Description: Pure source of K2O

Formula: K2O

Oxide Analysis Formula Tolerance
K2O 100.00% 1.00
Oxide Weight 94.20
Formula Weight 94.20

Related Information

Links

Materials Potassium Nitrate
Materials Pearl Ash
Typecodes Flux Source
Materials that source Na2O, K2O, Li2O, CaO, MgO and other fluxes but are not feldspars or frits. Remember that materials can be flux sources but also perform many other roles. For example, talc is a flux in high temperature glazes, but a matting agent in low temperatures ones. It can also be a flux, a filler and an expansion increaser in bodies.
Oxides K2O - Potassium Oxide

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy