1048 Frit

Alternate Names: 1048 Alkalifritte

Description: Alkaline frit

Oxide Analysis Formula Tolerance
CaO 1.07% 0.07
MgO 0.07% 0.01
K2O 7.87% 0.29
Na2O 11.19% 0.63
Al2O3 22.77% 0.78
B2O3 17.39% 0.88
SiO2 39.64% 2.32
Oxide Weight 351.07
Formula Weight 351.07

Notes

Was available in Norway, manufacturer unknown. Info from http://www.potters.org/subject70375.htm

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.
Typecodes Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types.