| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 51.00% | 0.75 | 3.0 |
| P2O5 | 42.00% | 0.25 | 1.5 |
| LOI | 7.50% | n/a | |
| Oxide Weight | 77.17 | ||
| Formula Weight | 85.27 | ||
Various brands contain:
Arsenic: 1-3 ppm
Fluoride: 30-750 ppm
Heavy metals: 10-150ppm
| Materials |
Tricalcium Phosphate
|
| Sieve Analysis Dry | on 100 mesh: 1.0% max on 200 mesh: 6.0% max |
|---|---|
| pH for dry powder | 5.9-7.1 |