Alternate Names: Tin(II) chloride
Formula: SnCl2
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SnO2 | 79.44% | 1.00 | |
| Cl | 20.56% | n/a | |
| Oxide Weight | 150.71 | ||
| Formula Weight | 189.72 | ||
This calculation does not have a balanced equation because the material itself does not have oxygen, this has to be taken from the kiln atmosphere during firing.
SnCl2 + O2 -> SnO2 + CL2
Weight of SnCl2 going into kiln: 189.7
Weight of SnO2 out in glaze
(O2 comes from atmosphere during firing): 150.7
2Cl lost during firing: 71
Percentage SnO2 is of original weight going in: 79.44
Remainder is LOI: 20.56
| URLs |
http://en.wikipedia.org/wiki/Tin%28II%29_chloride
Stannous Chloride at wikipedia |