1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

Stain (pink/coral)

Description: Coral/Pink Stains (ZrFe, ZrSiFe)

Notes

Color Range
-----------
Coral pink to pink shades.

Specific Gravity: 4.25-4.75
----------------

Stability/Kiln Atmosphere
-------------------------
Excellent in all types of glazes at temperatures up to over 1300C. The most stable of the known pink ceramic stains.

Compatibility
-------------
Suitable for blending with most other types of ceramic colors. Extensively used in blends with either zircon-vanadium blue, zircon-praseodymium yellow or tin-vanadium yellow to produce stable intermediate shades.

Cost
----
Moderate.

Note: This description is taken from information provided by Blythe Matthey and may or may not apply to stains of this family from other companies.

Related Information

Links

Oxide Analysis Formula Tolerance
Materials Stain
Typecodes Colorant
Metallic based materials that impart fired color to glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy