Sodium Feldspar 980

Description: Turkish Feldspar

Oxide Analysis Formula Tolerance
SiO2 71.00% 7.58
TiO2 0.28% 0.02
Al2O3 17.00% 1.07
Fe2O3 0.25% 0.01
Na2O 9.40% 0.97
K2O 0.40% 0.03
SO4 0.40%n/a
Oxide Weight 630.89
Formula Weight 633.42

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.
URLs http://ceramics.sibelcotools.com/tiles/porcelain-tiles/feldspar/
Sibelco Feldspar data

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy