Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Na2O | 17.80% | 1.00 | |
| Al2O3 | 5.10% | 0.17 | |
| SiO2 | 77.10% | 4.47 | |
| Oxide Weight | 348.31 | ||
| Formula Weight | 348.31 | ||
| Materials |
Eutectics
|
| Typecodes |
Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries. |
| Frit Softening Point | 800C |
|---|