Shigaraki Feldspar

Oxide Analysis Formula Tolerance
CaO 2.18% 0.27
K2O 4.71% 0.35
MgO 1.63% 0.29
Na2O 3.50% 0.40
Al2O3 14.44% 1.00
SiO2 72.24% 8.49
Fe2O3 0.53% 0.02
LOI 0.77%n/a
Oxide Weight 700.93
Formula Weight 706.37