Ratchaburi Soda Feldspar

Description: Thai feldspar from Rathcaburi City

Oxide Analysis Formula Tolerance
Fe2O3 0.16% 0.01
CaO 1.29% 0.14
Na2O 8.93% 0.86
K2O 0.10% 0.01
Al2O3 17.34% 1.01
SiO2 72.18% 7.15
Oxide Weight 594.92
Formula Weight 594.92

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy