Pyrotrol 2254

Description: Andalusite/Pyrophyllite Ore

Oxide Analysis Formula Tolerance
K2O 0.20% 0.01
Na2O 0.20% 0.02
Al2O3 20.00% 1.00
SiO2 75.00% 6.36
Fe2O3 0.60% 0.02
LOI 2.80%n/a
Oxide Weight 489.60
Formula Weight 503.70

Notes

Similar size and bulk density to 2253, but with slightly higher iron content.

Related Information

Links

Materials Pyrotrol
URLs https://www.rescoproducts.com/docs/default-source/data-sheets-us/sds/pyrotrol-all-grades-msds.pdf?sfvrsn=905bb13b_5
SDS for all versions of Pyrotrol
URLs https://www.rescoproducts.com/docs/default-source/data-sheets-us/pds/pyrotrol-2253-and-2254-and-3503.pdf
Pyrotrol Data Sheet

Data

Bulk Density lbs/cu. ft. (Packed) 45
Pyrometric Cone Equivalent 26
Sieve Analysis Dry +200 mesh: 1%

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy