Oct 22, 2026: We are working on protecting our servers against the PHP2Shell vulnerability just discovered. The CDN download server is back online. The digitalfire and insight-live servers were patched on Oct 21.

1-9 | A | B | C | D | E | F | Frits | G | H | I | J | K | L | M | N | O | P | Q | R | S | T | U | V | W | X | Y | Z

PuraFlow AK Ball Clay

Alternate Names: Blue Ball Clay

Description: Very high plastic buff burning Devon ball clay

Oxide Analysis Formula Tolerance
Al2O3 32.00% 1.00
SiO2 50.00% 2.65
K2O 1.00% 0.03
Fe2O3 1.10% 0.02
Na2O 1.10% 0.06
LOI 10.00%n/a
Oxide Weight 271.58
Formula Weight 301.75

Notes

LOI estimated

Related Information

Links

Typecodes Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites.

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy