Na & Ba Metasilicate Eutectic

Formula: BaSiO3 . 2.62Na2SiO3

Oxide Analysis Formula Tolerance
BaO 28.70% 0.28
Na2O 30.40% 0.72
SiO2 40.90% 1.00
Oxide Weight 147.59
Formula Weight 147.59

Related Information

Links

Glossary Eutectic
In ceramics, this term refers to certain chemistries that melt at much-lower-than-expected temperatures.
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 908C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy