Alternate Names: Madoc Spar, Madoc H Feldspar
Description: Legacy Potash feldspar
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| K2O | 8.89% | 0.62 | |
| Na2O | 3.59% | 0.38 | |
| Al2O3 | 17.39% | 1.12 | |
| SiO2 | 68.63% | 7.50 | |
| Oxide Weight | 646.85 | ||
| Formula Weight | 646.85 | ||
Another formula for Madoc:
K2O 0.61
Na2O 0.34
CaO 0.05
Al2O3 1.04
SiO2 6.4
| Materials |
Potash Feldspar
A feldspar having a KNaO content that predominates in potassium. |
| Materials |
Soda Feldspar
A feldspar having a KNaO content that predominates in sodium. |
| Typecodes |
Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies. |