| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 0.50% | 0.03 | |
| K2O | 1.10% | 0.04 | |
| MgO | 0.50% | 0.05 | |
| TiO2 | 1.30% | 0.06 | |
| Al2O3 | 27.50% | 1.00 | |
| SiO2 | 54.50% | 3.36 | |
| Fe2O3 | 1.20% | 0.03 | |
| LOI | 13.30% | n/a | |
| Oxide Weight | 321.21 | ||
| Formula Weight | 370.48 | ||
| Typecodes |
Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites. |