Alternate Names: 37 031,37-031
Description: Bleifreie Kalzium-Borat-Fritte
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 44.60% | 0.69 | |
| BaO | 55.40% | 0.31 | |
| Oxide Weight | 86.48 | ||
| Formula Weight | 86.48 | ||
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 85 x 10-7 |
|---|---|
| Frit Softening Point | 610C |
| Frit Melting Range (C) | 700-1150C |