Description: Pale brown burning plastic ball clay
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| SiO2 | 57.30% | 3.89 | |
| Al2O3 | 25.00% | 1.00 | |
| Fe2O3 | 2.00% | 0.05 | |
| TiO2 | 0.80% | 0.04 | |
| MgO | 0.40% | 0.04 | |
| CaO | 0.30% | 0.02 | |
| Na2O | 0.20% | 0.01 | |
| K2O | 2.00% | 0.09 | |
| LOI | 9.00% | n/a | |
| Oxide Weight | 359.04 | ||
| Formula Weight | 394.55 | ||
| Typecodes |
Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites. |
![]() PayPal | No tracking, No ads, No paywall, No transient content! Just organized, concise information constantly updated and improved. Was this helpful? Consider supporting me. |
| By Tony Hansen Follow me on ![]() | ![]() |
Buy me a coffee and we can talk