Description: Reimbold & Strick barium matte frit
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 12.00% | 0.36 | |
| CaO | 5.00% | 0.27 | |
| SiO2 | 51.00% | 2.60 | |
| BaO | 25.00% | 0.50 | |
| K2O | 7.00% | 0.23 | |
| Oxide Weight | 306.26 | ||
| Formula Weight | 306.26 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Typecodes |
Frit
A frit is the powdered form a man-made glass. Frits are premelted, then ground to a glass. They have tightly controlled chemistries, they are available for glazes of all types. |
| Co-efficient of Linear Expansion | 67 x 10-7 (20-400C) |
|---|---|
| Frit Softening Point | >800C |
| Glass Transition Temperature | 660C |