Description: Ball clay for casting slips
| Oxide | Analysis | Formula | Tolerance |
|---|
| Typecodes |
Ball Clay
Ball clays are abundant and very plastic and are used in all types of plastic forming bodies. They are not as white-burning or refractory as kaolins but lower in iron and fluxes than bentonites. |