Esan Feldspar

Alternate Names: ESF501FG

Description: Turkish Soda Feldspar

Oxide Analysis Formula Tolerance
SiO2 70.00% 6.66
Al2O3 18.00% 1.01
Fe2O3 0.05% -
TiO2 0.05% -
CaO 0.30% 0.03
MgO 0.20% 0.03
K2O 0.30% 0.02
Na2O 10.00% 0.92
LOI 0.30%n/a
Oxide Weight 565.84
Formula Weight 567.54

Related Information

Links

Typecodes Feldspar
The most common source of fluxes for high and medium temperature glazes and bodies.

Data

Ultimate Particle Size Distribution +200 3.50 +100 13.00 +74 24.50 +63 6.00 +45 13.00 -45 40.00

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy