Monthly Tech-Tip | No tracking! No ads! |
Description: High iron mineral
Oxide | Analysis | Formula | Tolerance |
---|---|---|---|
SiO2 | 13.40% | 1.17 | |
Al2O3 | 7.40% | 0.38 | |
Fe2O3 | 8.50% | 0.28 | |
FeO | 31.90% | 2.05 | |
MgO | 2.50% | 0.33 | |
CaO | 6.10% | 0.57 | |
P2O5 | 2.80% | 0.10 | |
H2O | 8.50% | n/a | |
CO2 | 17.40% | n/a | |
Oxide Weight | 381.10 | ||
Formula Weight | 514.30 |