Ceradel Frit C 1256

Alternate Names: Fritte C1256, Fritte C 1256, Ceradel Frit 1256

Description: Fritte borique, very low expansion borate frit

Oxide Analysis Formula Tolerance
SiO2 59.00% 7.07
Al2O3 8.00% 0.57
K2O 0.40% 0.03 .75
BaO 1.50% 0.07 2.5
B2O3 24.00% 2.48
CaO 7.00% 0.90
Oxide Weight 719.70
Formula Weight 719.70

Notes

We only have an approximate analysis from the manufacturer. Do you have a precise one?

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.

Data

Co-efficient of Linear Expansion 45 (10-7/C 20/300C)
Frit Softening Point 920-1020C M

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy