Alternate Names: Fritte C1254, Fritte C 1254, Ceradel Frit 1254
Description: Fritte calco-alcaline sans plomb
| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| Al2O3 | 7.38% | 0.20 | |
| B2O3 | 27.73% | 1.10 | |
| Na2O | 11.22% | 0.50 | |
| CaO | 10.15% | 0.50 | |
| SiO2 | 43.51% | 2.00 | |
| Oxide Weight | 276.30 | ||
| Formula Weight | 276.30 | ||
| Materials |
Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot. |
| Co-efficient of Linear Expansion | 72x10-7 (20/300C) |
|---|---|
| Frit Softening Point | 800-920C |