Ceradel Frit C 1252

Alternate Names: Fritte C1252, Fritte C 1252, Ceradel Frit 1252

Description: Fritte borocalcique sans plomb

Oxide Analysis Formula Tolerance
B2O3 22.57% 0.98
Al2O3 13.83% 0.41
CaO 15.21% 0.82
Na2O 1.85% 0.09
SiO2 43.73% 2.20
K2O 2.80% 0.09
Oxide Weight 302.37
Formula Weight 302.37

Related Information

Links

Materials Frit
Frits are made by melting mixes of raw materials, quenching the melt in water, grinding the pebbles into a powder. Frits have chemistries raw materials cannot.

Data

Co-efficient of Linear Expansion 58x10-7 (20/300C)
Frit Softening Point 900-980C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy