Calcium-Aluminum-Silicate Eutectic

Oxide Analysis Formula Tolerance
CaO 23.25% 1.00
Al2O3 14.75% 0.35
SiO2 62.00% 2.49
Oxide Weight 241.29
Formula Weight 241.29

Related Information

Links

Materials Eutectics
Typecodes Eutectic
These are theoretical mixtures of oxides, not real materials. Use these to learn about low melting chemistries.

Data

Frit Softening Point 1170C

PayPal
No tracking, No ads, No paywall, No transient content!
Just organized, concise information constantly updated and improved.
Was this helpful? Consider supporting me.
By Tony Hansen
Follow me on

Got a Question?

Buy me a coffee and we can talk

 



https://digitalfire.com, All Rights Reserved
Privacy Policy