| Oxide | Analysis | Formula | Tolerance |
|---|---|---|---|
| CaO | 1.50% | 1.72 | |
| MgO | 91.60% | 145.81 | |
| Al2O3 | 1.59% | 1.00 | |
| SiO2 | 4.00% | 4.27 | |
| Fe2O3 | 0.81% | 0.32 | |
| LOI | 0.50% | n/a | |
| Oxide Weight | 6,383.02 | ||
| Formula Weight | 6,415.09 | ||
| Typecodes |
Refractory
Materials that melt at high temperatures. These are normally used for kiln bricks, furniture, etc. or for ceramics that must withstand high temperatures during service. |